性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 |
吸水率 | 23.C 60%RH | ASTM D-570 | 0.22 | % |
熔體流動速率 | ASTM D-1237 | 9 | G/10min | ||
成型收縮率 | 平行方向 | 20 | % | ||
比重 | ASTM D-792 | 1.41 | |||
機械性能 | 拉伸強度 | 1.6mm | ASTM D-1822 | 98 | KJ/m2 |
拉伸長度 | 23℃ | ASTM D-638 | 50 | % | |
拉伸強度 | 23℃ | ASTM D-638 | 62.3 | MPa | |
撓曲強度 | 23℃ | ASTM D-790 | 91.2 | MPa | |
洛氏硬度 | ASTM D-785 | 80 | M scale | ||
IZOD沖擊強度 | 3.2mm | ASTM D-256 | 54 | J/m | |
彎曲模量 | 23℃ | ASTM D-790 | 2.62 | GPa | |
撕裂強度 | 2mm | ASTM D-732 | 54.9 | MPa | |
電氣性能 | 體積電阻系數(shù) | ASTM D-257 | 1×1014/ | ||
介電常數(shù) | 106Hz | ASTM D-150 | 33 | Pf/m | |
表面電阻系數(shù) | ASTM D-257 | 1×1016 | |||
介電損耗正切 | 106Hz | ASTM D-150 | 0.007 | ||
耐電壓 | ASTM D-149 | 19 | MV/m | ||
熱性能 | 燃燒性 | UL 94 | HB | ||
熔點 | 10℃/min | DSC | 165 | ℃ | |
負荷撓曲溫度 | 455kPa | ASTM D-648 | 158 | ℃ | |
負荷撓曲溫度 | 820kPa | ASTM D-648 | 110 | ℃ | |
線膨脹系數(shù) | 20℃-80℃ | ASTM D-696 | 13 | 10 |
POM F20-03 南通寶泰菱