PPS A504 日本東麗工業(yè)株式會(huì)社 物性數(shù)據(jù) |
①原料描述部分 |
|||
規(guī)格級(jí)別: |
玻璃纖維級(jí) |
外觀顏色: |
--- |
用途概述: |
--- |
||
備注說(shuō)明: |
特性:標(biāo)準(zhǔn)類型:玻璃纖維+礦物填充 |
②原料技術(shù)數(shù)據(jù) |
||||||||||||||
性能項(xiàng)目 |
試驗(yàn)條件[狀態(tài)] |
測(cè)試方法 |
測(cè)試數(shù)據(jù) |
數(shù)據(jù)單位 |
||||||||||
基本性能 |
吸水率 |
24hr,23℃于水中 |
ASTM D-570 |
0.02 |
% |
|||||||||
物理性能 |
比重 |
--- |
ASTM D-792 |
1.96 |
--- |
|||||||||
泰伯磨耗 |
--- |
ASTM D-D1044 |
70 |
mg/1000次 |
||||||||||
摩擦系數(shù)/對(duì)鐵 |
--- |
ASTM D-1894 |
0.30 |
--- |
||||||||||
限定PV值 |
--- |
TORAY |
815 |
kj/m2.hr |
||||||||||
|
--- |
|
|
|
||||||||||
機(jī)械性能 |
洛氏硬度 |
--- |
ASTM D-785 |
123 |
R |
|||||||||
拉伸強(qiáng)度 |
23℃ |
ASTM D-638 |
140 |
MPa |
||||||||||
延伸率 |
23℃ |
ASTM D-638 |
2.1 |
% |
||||||||||
彎曲強(qiáng)度 |
23℃ |
ASTM D-790 |
200 |
MPa |
||||||||||
彎曲模量 |
23℃ |
ASTM D-790 |
17.6 |
GPa |
||||||||||
壓縮強(qiáng)度 |
--- |
ASTM D-732 |
60 |
--- |
||||||||||
|
--- |
|
|
|
||||||||||
電氣性能 |
阻燃性 |
--- |
--- |
V-0 |
UL-94 |
|||||||||
抗電弧性 |
--- |
ASTM D-495 |
180 |
Second |
||||||||||
體積電阻 |
--- |
ASTM D-257 |
1016 |
Ω.m |
||||||||||
介電強(qiáng)度 |
--- |
ASTM D-150 |
15 |
MV/m |
||||||||||
介電常數(shù) |
106Hz |
ASTM D-150 |
5.8 |
--- |
||||||||||
損耗因子 |
106Hz |
ASTM D-150 |
0.002 |
--- |
||||||||||
熱 性 能 |
|
--- |
|
|
|
|||||||||
熔點(diǎn) |
--- |
DSC |
278 |
°C |
||||||||||
熱變形溫度 |
1.82MPa |
ASTM D-648 |
>260 |
℃ |
||||||||||
其它性能 |
流動(dòng)長(zhǎng) |
320℃,98MPa |
TORAY |
90 |
×10-3m |