性能項(xiàng)目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ? | ASTM D638/ISO 527 | 40 | kg/cm2(MPa)[Lb/in2] |
拉伸模量 | ? | ASTM D638/ISO 527 | ? | kg/cm2(MPa)[Lb/in2] | |
拉伸屈服伸長率(延伸率) | ? | ASTM D638/ISO 527 | ? | % | |
拉伸斷裂伸長率(延伸率) | ? | ASTM D638/ISO 527 | 500 | % | |
彎曲模量(彎曲彈性率) | ? | ASTM D790/ISO 178 | 207 | kg/cm2(MPa)[Lb/in2] | |
彎曲強(qiáng)度 | ? | ASTM D790/ISO 178 | ? | kg/cm2(MPa)[Lb/in2] | |
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | ? | kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 | ? | kg·cm/cm(J/M)ft·lb/in | ||
1/8" 23℃ | ASTM D256/ISO 179 | ? | kg·cm/cm(J/M)ft·lb/in | ||
1/8" -30℃ | ASTM D256/ISO 179 | ? | kg·cm/cm(J/M)ft·lb/in | ||
硬度 A | ? | ASTM D2240/ISO 868 | ? | Shore A | |
硬度 D | ? | ASTM D2240/ISO 868 | ? | Shore D | |
撕裂強(qiáng)度 | ? | ASTM D624/ISO 34 | 158 | Mpa/Psi | |
物性性能 | 比重(密度) | ? | ASTM D792/ISO 1183 | 1.20 | ? |
熔融指數(shù)(流動系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | 18 | g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 | ? | g/10min | ||
丁二烯/本乙 ?烯比例 | ? | ASTM D1416 | ? | % | |
油含量 | ? | ASTM D1416 | ? | phr | |
揮發(fā)份 | ? | ASTM D1416 | ? | wt./% | |
灰份 | ? | ASTM D1416 | ? | wt./% | |
熱性能 | 維卡軟化點(diǎn) | ? | ASTM D1525/ISO R306 | 180 | ℃(℉) |
熔點(diǎn) | ? | - | 203 | ℃(℉) | |
玻璃化溫度 | ? | ? | ? | ℃(℉) | |
光學(xué)性能 | 透光率 | ? | ASTM D1003/ISO 13468 | ? | % |
光澤度 | ? | ASTM D2457 | ? | ? | |
加工條件 | 干燥條件 | ? | ? | ? | ? |
加工溫度 | 射嘴 | ? | ? | ℃ | |
料筒前段 | ? | ? | ℃ | ||
料筒中段 | ? | ? | ℃ | ||
料筒后段 | ? | ? | ℃ | ||
熔體溫度 | ? | ? | ? | ℃ | |
模具溫度 | ? | ? | ? | ℃ | |
壓力 | 注塑壓力 | ? | ? | Mpa | |
保壓壓力 | ? | ? | Mpa | ||
背壓 | ? | ? | Mpa | ||
螺桿轉(zhuǎn)速 | ? | ? | ? | rpm | |
其他 | 備注 | ? | |||
顏色 | ? | ||||
特性 | ? | ||||
用途 |
? |
TPE 美國杜邦 7246 高強(qiáng)度 耐高溫