原料技術(shù)數(shù)據(jù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
物理性能 | 模塑收縮量 | Flow | ASTM D 955 | 0.005-0.007 | cm/cm | |
熔體流動(dòng)速率 | cm3/10min,melt volume rate,MVR at 260C/5.0 kg | ISO 1133 | 16 | g/10min | ||
粘度 | MV,260 C,1500 1/sec | DIN 54811 | 311000 | cP | ||
含濕量(大) | 23℃ | ISO 62 | 0.6 | % | ||
吸濕率(平衡) | (23 C/50%RH)1L | ISO 15512 | 0.2 | % | ||
密度 | - | ASTM D 792 | 1.2 | g/cc | ||
- | ISO 1183 | 1.2 | g/cc | |||
機(jī)械性能 | 抗拉強(qiáng)度 | Ultimate | 5 mm/min | ISO 527 | 45 | MPa |
Yield | 50 mm/min | ISO 527 | 50 | MPa | ||
Ultimate | 5 mm/min | ISO 527 | 50 | MPa | ||
Yield | 50 mm/min | ISO 527 | 60 | MPa | ||
卻貝沖擊值 | 缺口低溫 | at-30C,V-notch Edgew 80*10*4 sp=62 | ISO 179/1eA | 1.9 | J/m | |
缺口 | 23C,V-notch Edgew 80*10*4 sp=62 | ISO 179/1eA | 4.7 | J/m | ||
拉伸模量 | 1mm/min | ISO 527 | 2.6 | GPa | ||
IZOD沖擊值 | 缺口 | 80*10*4+23C | ISO 178/1A | 46 | kJ/m | |
無缺口 | 80*10*4+23C | ISO 178/1U | NB | - | ||
無缺口低溫 | 80*10*4-30C | ISO 178/1U | NB | - | ||
缺口低溫 | 80*10*4-30C | ISO 178/1A | 17 | kJ/m | ||
撓曲模量 | 2mm/min | ISO 178 | 2.5 | GPa | ||
屈服撓曲強(qiáng)度 | 2mm/min | ISO 178 | 85 | MPa | ||
硬度 | Rockwell R | ISO 2039/2 | 123 | - | ||
H358/30 | ISO 2039/1 | 104 | MPa | |||
泰伯磨耗值 | CS-17,1kg | GE Test | 62 | |||
拉伸率 | 斷裂 | 50 mm/min | ISO 527 | Min 50 | % | |
斷裂 | 5 mm/min | ISO 527 | 60 | % | ||
屈服 | 5 mm/min | ISO 527 | 4 | % | ||
屈服 | 50 mm/min | ISO 527 | 4 | % | ||
電氣性能 | 比較性漏電指數(shù) | IEC 60112/3rd | 250 | V | ||
表面電阻率 | ROA | IEC 60093 | Min 1e+015 | Ohm | ||
體積電阻率 | IEC 60093 | Min 1e+015 | Ohm-cm | |||
電弧電阻 | Tungsten | ASTM D 495 | 5 | sec | ||
介電強(qiáng)度 | in oil,3.2mm | IEC 60243-1 | 17 | kv/mm | ||
in oil,1.6mm | IEC 60243-1 | 25 | kv/mm | |||
in oil,0.8mm | IEC 60243-1 | 35 | kv/mm | |||
介電常數(shù) | 1 MHz | IEC 60250 | 2.6 | |||
50 Hz | IEC 60250 | 3 | ||||
介電損耗因數(shù) | 50 Hz | IEC 60250 | 0.005 | |||
1 MHz | IEC 60250 | 0.008 | ||||
熱性能 | 可燃性 | 1.5mm | UL 94 | V-0 | ||
94-5VB at 2mm | UL 94 | V-0 | ||||
灼熱絲試驗(yàn) | passes at 1mm | IEC 60695-2-1 | 960 | ℃ | ||
維卡軟化點(diǎn) | B/50 | ISO 306 | 136 | ℃ | ||
B/120 | ISO 306 | 138 | ℃ | |||
導(dǎo)熱率 | ISO 8302 | 0.2 | W/m-K | |||
含氧指數(shù) | ISO 4589 | 32 | % | |||
熱畸變溫度 | at 0.46MPa(66psi) | HDT/Be,0.45MPa Edgew 120*10*4 sp=100mm | ISO 75/Be | 128 | ℃ | |
at 1.8MPa(264psi) | HDT/Ae,1.82MPa Edgew 120*10*4 sp=100mm | ISO 75/Ae | 112 | ℃ | ||
UL熱指數(shù) | 電性能 | UL 746B | 125 | ℃ | ||
機(jī)械沖擊性能 | UL 746B | 60 | ℃ | |||
非機(jī)械沖擊性能 | UL 746B | 115 | ℃ | |||
可燃性測(cè)試 | mm,IEC Needle Flame Test,10s,passes at | IEC 60695-2-2 | 1.6 | |||
其它性能 | 球體壓力測(cè)試 | 125C+/-2C | IEC 60035-1 | passes |